General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.92 g/cm³ Show Material materials with Densidad of 0.92 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 53 [-] Show Material materials with Dureza Shore D of 53 [-] | ISO 868 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.2 [-] Show Material materials with Constante dieléctrica of 2.2 [-] | ASTM D150 | at 60 Hz |
Factor de disipación | 23.0 °C | 5E-4 [-] Show Material materials with Factor de disipación of 5E-4 [-] | ASTM D150 | at 60 Hz |
Resistividad eléctrica | 23.0 °C | 8.50E+13 Ω·m Show Material materials with Resistividad eléctrica of 8.50E+13 Ω·m | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | It is used for wire and cable applications (telecommunication and power cable (LV, MV, HV) jacketing, halogen-free flame retardant (HFFR) compounds, one-step or two-steps silane crosslinkable for cable insulation). |