General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.92 g/cm³ Show Material materials with Densidad of 0.92 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 53 [-] Show Material materials with Dureza Shore D of 53 [-] | ISO 868 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 121 °C Show Material materials with Temperatura de fusión of 121 °C | SABIC method |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.2 [-] Show Material materials with Constante dieléctrica of 2.2 [-] | ASTM D150 | at 60 Hz |
Factor de disipación | 23.0 °C | 5E-4 [-] Show Material materials with Factor de disipación of 5E-4 [-] | ASTM D150 | at 60 Hz |
Resistividad eléctrica | 23.0 °C | 8.50E+13 Ω·m Show Material materials with Resistividad eléctrica of 8.50E+13 Ω·m | ASTM D257 |
Rigidez dieléctrica | 23.0 °C | 55 kV/mm Show Material materials with Rigidez dieléctrica of 55 kV/mm | ASTM D149 | at 500 V/sec |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable |