General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.11 % Show Material materials with Absorción de agua of 0.11 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.44 g/cm³ Show Material materials with Densidad of 1.44 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Material materials with Elongación of 2 % | ISO 527 | 5 mm/min |
Módulo de flexión | 23.0 °C | 7 GPa Show Material materials with Módulo de flexión of 7 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 9 GPa Show Material materials with Módulo elástico of 9 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 130 MPa Show Material materials with Resistencia a la flexión of 130 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 100 MPa Show Material materials with Resistencia a la tracción of 100 MPa | ISO 527 | 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 5 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | ISO 179/1eA |
23.0 °C | 6 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30.0 °C | 40 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | ISO 179/1eU |
23.0 °C | 40 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | ISO 179/1eU | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 6 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A |
23.0 °C | 7 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 7 kJ/m² | ISO 180/1A | |
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 35 kJ/m² | ISO 180/1U |
23.0 °C | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 35 kJ/m² | ISO 180/1U | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.5E-5 1/K | ISO 11359-2 | -23°C to 80°C | ||
Conductividad térmica | 23.0 °C | 0.22 W/(m·K) Show Material materials with Conductividad térmica of 0.22 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 1.80 MPa | 139 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 139 °C | ISO 75/Ae | 1.8 MPa | |||
Relative temperature index, electrical | 130 °C Show Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 125 °C Show Material materials with Relative temperature index, mechanical impact of 125 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 145 °C Show Material materials with Temperatura de reblandecimiento Vicat of 145 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating | 1.5mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.1 [-] Show Material materials with Constante dieléctrica of 3.1 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 0.01 [-] Show Material materials with Factor de disipación of 0.01 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 16 kV/mm Show Material materials with Rigidez dieléctrica of 16 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.4 % Show Material materials with Contracción of 0.1 - 0.4 % | SABIC method |
Velocidad de flujo del volumen derretido | 5 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 5 cm³/10min | ISO 1133 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors,Audio,Circuit Protection,Data Management,Data Transfer,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Heavy Vehicles,Lab Ware and Clinical Diagnostics,Lawn/Garden,Medical Device,Meter Water,Monitoring and Imaging,Non-LED Lighting,Personal Computing,Pharmaceutical Manufacturing,Pharmaceutical Packaging & Drug Delivery,Power Boat,Small Appliance,Surgical Devices,Watch/Jewelry,Wearables,Wireless Communications,Wiring Devices | |
Fillers | 30% Glass Fiber | |
Processing methods | Drying Temperature: 120°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 290-320°C, Nozzle Temperature: 280-310°C, Front - Zone 3 Temperature: 290-320°C, Middle - Zone 2 Temperature: 280-310°C, Rear - Zone 1 Temperature: 270-300°C, Hopper Temperature: 60-80°C, Mold Temperature: 80-120°C |