General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Material materials with Absorción de agua of 0.15 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.26 g/cm³ Show Material materials with Densidad of 1.26 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 6 % Show Material materials with Elongación of 6 % | ASTM D 638 | Type I, 5 mm/min | ||
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ASTM D 638 | Type I, 5 mm/min | ||
Flexural yield strength | 23.0 °C | 122 MPa Show Material materials with Flexural yield strength of 122 MPa | ISO 178 | 2 mm/min | ||
Impact strength, Izod notched, ASTM | -30.0 °C | 70 J/m Show Material materials with Impact strength, Izod notched, ASTM of 70 J/m | ASTM D 256 | ||
23.0 °C | 90 J/m Show Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 | |||
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1200 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 1200 J/m | ASTM D 4812 | ||
Límite elástico | 23.0 °C | 74 MPa Show Material materials with Límite elástico of 74 MPa | ASTM D 638 | Type I, 5 mm/min | ||
Módulo de flexión | 23.0 °C | 3.5 GPa Show Material materials with Módulo de flexión of 3.5 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 3.6 GPa Show Material materials with Módulo elástico of 3.6 GPa | ASTM D 638 | 5 mm/min | ||
Resistencia a la tracción | 23.0 °C | 62 MPa Show Material materials with Resistencia a la tracción of 62 MPa | ASTM D 638 | Type I, 5 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 7 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | ISO 179/1eA | ||
23.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA | |||
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | ||
23.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | |||
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 73 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 73 kJ/m² | ISO 180/1U | ||
Resistencia al choque, ensayo Charpy no entallado | No Break @ 23,-30°C | ISO 179/1eU |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 5E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 7.4E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 137 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 137 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Temperatura de reblandecimiento Vicat | 149 °C Show Material materials with Temperatura de reblandecimiento Vicat of 149 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Compliant, 94-5VB Rating | 3mm | UL 94 by SABIC-IP |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 175 V Show Material materials with Índice de seguimiento comparativo of 175 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción of 0.4 - 0.6 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 8 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 8 g/10min | ASTM D 1238 | 300°C/1.2 kg | |
Velocidad de flujo del volumen derretido | 7 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 7 cm³/10min | ISO 1133 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | ATM/Ticket Machine,Circuit Protection,Data Transfer,Displays,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Heavy Vehicles,Lab Ware and Clinical Diagnostics,LED Lighting,Medical Device,Monitoring and Imaging,Non-LED Lighting,Personal Computing,Power Boat,Power Manangement,Small Appliance,Wireless Communications,Wiring Devices | |
Fillers | 10% Glass Fiber | |
Processing methods | Drying Temperature: 120°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 290-320°C, Nozzle Temperature: 280-310°C, Front - Zone 3 Temperature: 290-320°C, Middle - Zone 2 Temperature: 280-310°C, Rear - Zone 1 Temperature: 270-300°C, Hopper Temperature: 60-80°C, Mold Temperature: 80-120°C |