General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.9 g/cm³ Show Material materials with Densidad of 0.9 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation at yield | 23.0 °C | 4.5 % Show Material materials with Elongation at yield of 4.5 % | ISO 527-1/-2 |
Hardness, Rockwell L | 23.0 °C | 98 [-] Show Material materials with Hardness, Rockwell L of 98 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | -20.0 °C | 32 J/m Show Material materials with Impact strength, Izod notched, ASTM of 32 J/m | ASTM D256 |
23.0 °C | 53 J/m Show Material materials with Impact strength, Izod notched, ASTM of 53 J/m | ASTM D256 | |
Límite elástico | 23.0 °C | 26 MPa Show Material materials with Límite elástico of 26 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 1.35 GPa Show Material materials with Módulo de flexión of 1.35 GPa | ASTM D790 A |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Thin wall packaging |