Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation at yield | 23.0 °C | 8 % Show Material materials with Elongation at yield of 8 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 103 [-] Show Material materials with Hardness, Rockwell L of 103 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 30 J/m Show Material materials with Impact strength, Izod notched, ASTM of 30 J/m | ASTM D256 |
Límite elástico | 23.0 °C | 38 MPa Show Material materials with Límite elástico of 38 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 2 GPa Show Material materials with Módulo de flexión of 2 GPa | ASTM D790 A |
Aplicaciones térmicas
Óptico
Property | Value | Comment |
---|---|---|
Turbidez | 17 % Show Material materials with Turbidez of 17 % | ASTM D 1003 |
Technological properties
Property | ||
---|---|---|
Application areas | Sheet |