Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
SABIC® PP 5770N
SABIC® PP 5770N is a PP homopolymer grade with antistatic and nucleating agents. It is suitable for producing injection molded applications with outstanding flow properties, good dimensional stability, high stiffness, excellent organoleptic properties and good clarity comparing to the regular PP homopolymer grades. SABIC® PP 5770N encompasses the following features: very high top load strength & down gauging potential; isotropy shrinkage performance (dimensional stability); high crystallization temperature and superior flow behavior (lower cycle time); easy mold filing for aesthetic & large items; clean product in combination of low / no odor & taste.
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationMecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation at yield | 23.0 °C | 7 % Show Material materials with Elongation at yield of 7 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 98 [-] Show Material materials with Hardness, Rockwell L of 98 [-] | ASTM D785 |
Límite elástico | 23.0 °C | 40 MPa Show Material materials with Límite elástico of 40 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 1.68 GPa Show Material materials with Módulo de flexión of 1.68 GPa | ASTM D790 A |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de reblandecimiento Vicat | 150 °C Show Material materials with Temperatura de reblandecimiento Vicat of 150 °C | ASTM D1525 |
Technological properties
Property | ||
---|---|---|
Application areas | Houseware & appliances |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.