Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
SABIC® SUPEER™ 7118NE
SABIC® SUPEER™ 7118NE is a metallocene ethylene-hexene copolymer. It has a good processability and performs well in a wide range of general purpose and high performance blown film applications. Films produced with this grade offer good tensile and impact strength, puncture resistance and sealing properties. SABIC® SUPEER™ 7118NE is typically used for applications like heavy duty bags, agriculture film, stretch hood, lamination film, frozen bags. Properties have been measured on blown film of 25 µm and BUR = 2.5 Typical processing conditions for SABIC® SUPEER™ 7118NE : processing temperatures 180 - 230 °C Blow up ratio: 2.0 - 4.0 This product is not intended for and must not be used in any pharmaceutical/medical applications.
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyethylene Wax: Uses and Properties
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationMecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Resistencia a desgarros | 23.0 °C | 117.6 kN/m Show Material materials with Resistencia a desgarros of 117.6 kN/m | ASTM D1922 |
Resistencia a desgarros transversal | 23.0 °C | 176.4 kN/m Show Material materials with Resistencia a desgarros transversal of 176.4 kN/m | ASTM D1922 |
Óptico
Property | Value | Comment |
---|---|---|
Turbidez | 20 % Show Material materials with Turbidez of 20 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | Heavy duty bags, agriculture film, stretch hood, lamination film, frozen bags. |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.