General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.96 g/cm³ Show Material materials with Densidad of 0.96 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 66 [-] Show Material materials with Dureza Shore D of 66 [-] | ASTM D2240 |
Elongación | 23.0 °C | 500 % Show Material materials with Elongación of 500 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 150 J/m Show Material materials with Impact strength, Izod notched, ASTM of 150 J/m | ASTM D256 |
Límite elástico | 23.0 °C | 30 MPa Show Material materials with Límite elástico of 30 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 1.1 GPa Show Material materials with Módulo de flexión of 1.1 GPa | ISO 178/1A |
Resistencia a la flexión | 23.0 °C | 28 MPa Show Material materials with Resistencia a la flexión of 28 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 18 MPa Show Material materials with Resistencia a la tracción of 18 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de reblandecimiento Vicat | 127 °C Show Material materials with Temperatura de reblandecimiento Vicat of 127 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 0.7 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 0.7 g/10min | ASTM D1238 | 190°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Dairy products, Juice Packaging |