General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.95 g/cm³ Show Material materials with Densidad of 0.95 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation at yield | 23.0 °C | 10 % Show Material materials with Elongation at yield of 10 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 26 MPa Show Material materials with Límite elástico of 26 MPa | ASTM D638 |
Módulo elástico | 23.0 °C | 1.05 GPa Show Material materials with Módulo elástico of 1.05 GPa | ASTM D638 |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 36 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 36 kJ/m² | ISO 179 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 6.5 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 6.5 g/10min | ISO 1133 | 190°C/21.6 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Jerry cans |