General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.96 g/cm³ Show Material materials with Densidad of 0.96 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 64 [-] Show Material materials with Dureza Shore D of 64 [-] | ASTM D2240 |
Elongation at yield | 23.0 °C | 7.5 % Show Material materials with Elongation at yield of 7.5 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 28 MPa Show Material materials with Límite elástico of 28 MPa | ISO 527-1/-2 |
Módulo elástico | 23.0 °C | 1.35 GPa Show Material materials with Módulo elástico of 1.35 GPa | ASTM D638 |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 6.5 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 6.5 kJ/m² | ISO 179 |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 75 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 75 kJ/m² | ISO 8256 |
Technological properties
Property | ||
---|---|---|
Application areas | Bottles |