General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Material materials with Absorción de agua of 0.15 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.16 g/cm³ Show Material materials with Densidad of 1.16 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 96.3 % Show Material materials with Elongación of 96.3 % | ASTM D 638 | Type I, 50 mm/min |
Elongation at yield | 23.0 °C | 4.7 % Show Material materials with Elongation at yield of 4.7 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 94 MPa Show Material materials with Flexural yield strength of 94 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 600 J/m Show Material materials with Impact strength, Izod notched, ASTM of 600 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 63 MPa Show Material materials with Límite elástico of 63 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.36 GPa Show Material materials with Módulo de flexión of 2.36 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.67 GPa Show Material materials with Módulo elástico of 2.67 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 51 MPa Show Material materials with Resistencia a la tracción of 51 MPa | ASTM D 638 | Type I, 50 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 105 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 105 °C | ASTM D 648 | 0.45 MPa, 3.2 mm | |||
Relative temperature index, electrical | 80 °C Show Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 111 °C Show Material materials with Temperatura de reblandecimiento Vicat of 111 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating | 0.8mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3 [-] Show Material materials with Constante dieléctrica of 3 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 0.01 [-] Show Material materials with Factor de disipación of 0.01 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 27 kV/mm Show Material materials with Rigidez dieléctrica of 27 kV/mm | ASTM D 149 | in oil, 1.6 mm |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción transversal of 0.5 - 0.7 % | SABIC method |
Velocidad de flujo de la masa derretida | 25.2 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 25.2 g/10min | ASTM D 1238 | 300°C/1.2 kg | |
Velocidad de flujo del volumen derretido | 23 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 23 cm³/10min | ISO 1133 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management,Data Transfer,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Heavy Vehicles,LED Lighting,Medical Device,Personal Computing,Photovoltaic Components,Power Manangement,Small Appliance,Wearables,Wireless Communications,Wiring Devices | |
Processing methods | Drying Temperature: 90°C, Drying Time: 4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 280-300°C, Nozzle Temperature: 270-290°C, Front - Zone 3 Temperature: 280-300°C, Middle - Zone 2 Temperature: 270-290°C, Rear - Zone 1 Temperature: 260-280°C, Hopper Temperature: 60-80°C, Mold Temperature: 90°C |