General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Material materials with Absorción de agua of 0.1 % | ASTM D 570 | 24 Hours |
Absorción de agua, equilibrio | 23.0 °C | 0.4 % Show Material materials with Absorción de agua, equilibrio of 0.4 % | ASTM D 570 |
Densidad | 23.0 °C | 1.17 g/cm³ Show Material materials with Densidad of 1.17 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 50 % Show Material materials with Elongación of 50 % | ASTM D 638 | Type I, 50 mm/min |
Elongation at yield | 23.0 °C | 5 % Show Material materials with Elongation at yield of 5 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 96 MPa Show Material materials with Flexural yield strength of 96 MPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Material materials with Hardness, Rockwell R of 120 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 427 J/m Show Material materials with Impact strength, Izod notched, ASTM of 427 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 58 MPa Show Material materials with Límite elástico of 58 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.68 GPa Show Material materials with Módulo de flexión of 2.68 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 2.68 GPa Show Material materials with Módulo elástico of 2.68 GPa | ASTM D 638 | 50 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.2E-5 1/K | ASTM E 831 | -40°C to 60°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 7.2E-5 1/K | ASTM E 831 | -40°C to 60°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Material materials with Conductividad térmica of 0.2 W/(m·K) | ASTM C177 | ||
Heat deflection temperature, 1.80 MPa | 80 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 80 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed | |||
Relative temperature index, electrical | 80 °C Show Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 70 °C Show Material materials with Relative temperature index, mechanical impact of 70 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 90 °C Show Material materials with Temperatura de reblandecimiento Vicat of 90 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94-5VB Flame Class Rating | 2.31mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3 [-] Show Material materials with Constante dieléctrica of 3 [-] | ASTM D 150 | at 100 Hz |
Factor de disipación | 23.0 °C | 4.8E-3 [-] Show Material materials with Factor de disipación of 4.8E-3 [-] | ASTM D 150 | at 50/60 Hz |
Resistividad eléctrica | 23.0 °C | 1.00E+15 Ω·m Show Material materials with Resistividad eléctrica of 1.00E+15 Ω·m | ASTM D 257 |
Rigidez dieléctrica | 23.0 °C | 17.9 kV/mm Show Material materials with Rigidez dieléctrica of 17.9 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 1 V Show Material materials with Índice de seguimiento comparativo of 1 V | UL 746A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción of 0.4 - 0.6 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción transversal of 0.4 - 0.6 % | SABIC method |
Velocidad de flujo de la masa derretida | 16 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 16 g/10min | ASTM D 1238 | 260°C/2.16 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning,Amusement Machine,ATM/Ticket Machine,Audio,Building Accessory,Circuit Protection,Data Management,Data Transfer,Dishwasher,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Freezer,Furnace/Heater,Heavy Vehicles,Infotainment/Telematic,Lab Ware and Clinical Diagnostics,Laundry Dryer,LED Lighting,Medical Device,Meter Gas,Monitoring and Imaging,Non-LED Lighting,Personal Computing,Pharmaceutical Packaging & Drug Delivery,Power Manangement,Refrigerator,Sail Boat,Security/Detection,Small Appliance,Surgical Tray,Trim,Vacuum Cleaner,Vending Machine,Washing Machine,Wearables,Wireless Communications,Wiring Devices | |
Processing methods | Drying Temperature: 75-80°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.04%, Melt Temperature: 230-275°C, Nozzle Temperature: 230-275°C, Front - Zone 3 Temperature: 225-275°C, Middle - Zone 2 Temperature: 215-260°C, Rear - Zone 1 Temperature: 210-255°C, Mold Temperature: 50-70°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 30-80%, Vent Depth: 0.038-0.076mm |