General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.2 % Show Material materials with Absorción de agua of 0.2 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.17 g/cm³ Show Material materials with Densidad of 1.17 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 65 % Show Material materials with Elongación of 65 % | ISO 527 | 5 mm/min | ||
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ISO 527 | 50 mm/min | ||
Flexural yield strength | 23.0 °C | 90 MPa Show Material materials with Flexural yield strength of 90 MPa | ISO 178 | 2 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 116 MPa Show Material materials with Hardness, Ball Indentation of 116 MPa | ISO 2039-1 | ||
Hardness, Rockwell R | 23.0 °C | 123 [-] Show Material materials with Hardness, Rockwell R of 123 [-] | ISO 2039-2 | ||
Límite elástico | 23.0 °C | 60 MPa Show Material materials with Límite elástico of 60 MPa | ISO 527 | 50 mm/min | ||
Módulo de flexión | 23.0 °C | 2.7 GPa Show Material materials with Módulo de flexión of 2.7 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.8 GPa Show Material materials with Módulo elástico of 2.8 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la tracción | 23.0 °C | 50 MPa Show Material materials with Resistencia a la tracción of 50 MPa | ISO 527 | 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 15 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | ISO 179/1eA | ||
23.0 °C | 45 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 45 kJ/m² | ISO 179/1eA | |||
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 14 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 14 kJ/m² | ISO 180/1A | ||
23.0 °C | 44 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 44 kJ/m² | ISO 180/1A | |||
Resistencia al choque, ensayo Charpy no entallado | No Break @ 23,-30°C | ISO 179/1eU | ||||
Resistencia al choque, ensayo Izod no entallado | No Break @ 23,-30°C| ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 1.80 MPa | 90 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 90 °C | ISO 75/Ae | 1.8 MPa | |||
Relative temperature index, electrical | 85 °C Show Material materials with Relative temperature index, electrical of 85 °C | UL 746B | |||
Relative temperature index, mechanical impact | 85 °C Show Material materials with Relative temperature index, mechanical impact of 85 °C | UL 746B | |||
Relative temperature index, mechanical strength | 85 °C Show Material materials with Relative temperature index, mechanical strength of 85 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 112 °C Show Material materials with Temperatura de reblandecimiento Vicat of 112 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94-5VB Flame Class Rating | 2.5mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.8 [-] Show Material materials with Constante dieléctrica of 2.8 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 6E-3 [-] Show Material materials with Factor de disipación of 6E-3 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 17 kV/mm Show Material materials with Rigidez dieléctrica of 17 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción of 0.4 - 0.6 % | SABIC method |
Velocidad de flujo del volumen derretido | 12 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 12 cm³/10min | ISO 1133 | 260°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning,Air Filtration,ATM/Ticket Machine,Audio,Auto Aftermarket,Building Accessory,Building Element,Circuit Protection,City,Data Management,Data Transfer,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Fluid Delivery,Food Processor,Food Transportation,Freezer,Furnace/Heater,Heavy Vehicles,Individual Equiptment,Lab Ware and Clinical Diagnostics,Laundry Dryer,Lawn/Garden,LED Lighting,Medical Device,Medical Facility Infrastructure,Meter Gas,Monitoring and Imaging,Motorcycle,Non-LED Lighting,Personal Care,Personal Computing,Photovoltaic Components,Power Manangement,Refrigerator,Renal and Blood Handling,Respiratory,Security/Detection,Small Appliance,Surgical Devices,Vacuum Cleaner,Washing Machine,Wearables,Wireless Communications,Wiring Devices | |
Processing methods | Drying Temperature: 90-100°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-280°C, Nozzle Temperature: 230-270°C, Front - Zone 3 Temperature: 240-280°C, Middle - Zone 2 Temperature: 230-270°C, Rear - Zone 1 Temperature: 210-240°C, Hopper Temperature: 60-80°C, Mold Temperature: 60-90°C |