General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Material materials with Absorción de agua of 0.1 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.28 g/cm³ Show Material materials with Densidad of 1.28 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 80 % Show Material materials with Elongación of 80 % | ASTM D 638 | Type I, 5 mm/min |
Elongation at yield | 23.0 °C | 4.9 % Show Material materials with Elongation at yield of 4.9 % | ASTM D 638 | Type I, 5 mm/min |
Flexural yield strength | 23.0 °C | 106 MPa Show Material materials with Flexural yield strength of 106 MPa | ISO 178 | 2 mm/min |
Hardness, Rockwell R | 23.0 °C | 98 [-] Show Material materials with Hardness, Rockwell R of 98 [-] | ISO 2039-2 |
Impact strength, Izod notched, ASTM | -30.0 °C | 90 J/m Show Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 |
23.0 °C | 500 J/m Show Material materials with Impact strength, Izod notched, ASTM of 500 J/m | ASTM D 256 | |
Límite elástico | 23.0 °C | 64 MPa Show Material materials with Límite elástico of 64 MPa | ASTM D 638 | Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 3.56 GPa Show Material materials with Módulo de flexión of 3.56 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 3.57 GPa Show Material materials with Módulo elástico of 3.57 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 50 MPa Show Material materials with Resistencia a la tracción of 50 MPa | ASTM D 638 | Type I, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA |
23.0 °C | 45 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 45 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A |
23.0 °C | 45 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 45 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 5.7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Conductividad térmica | 23.0 °C | 0.3 W/(m·K) Show Material materials with Conductividad térmica of 0.3 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 1.80 MPa | 90 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 90 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Relative temperature index, electrical | 60 °C Show Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 106 °C Show Material materials with Temperatura de reblandecimiento Vicat of 106 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94-5VB Flame Class Rating | 1.5mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.9 [-] Show Material materials with Constante dieléctrica of 2.9 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 4E-3 [-] Show Material materials with Factor de disipación of 4E-3 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 17 kV/mm Show Material materials with Rigidez dieléctrica of 17 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 250 V Show Material materials with Índice de seguimiento comparativo of 250 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción of 0.4 - 0.6 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 11.5 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 11.5 g/10min | ASTM D 1238 | 260°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 9 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 9 cm³/10min | ISO 1133 | 260°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures,Energy Management,Wiring Devices | |
Fillers | Mineral Powder | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Minimum Moisture Content: 0.04%, Melt Temperature: 220-245°C, Barrel - Zone 1 Temperature: 180-225°C, Barrel - Zone 2 Temperature: 190-230°C, Barrel - Zone 3 Temperature: 205-240°C, Barrel - Zone 4 Temperature: 210-245°C, Adapter Temperature: 210-245°C, Die Temperature: 210-245°C, Roll Stack Temp - Top: 70-100°C, Roll Stack Temp - Middle: 70-95°C, Roll Stack Temp - Bottom: 65-90°C |