Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.2 % Show Material materials with Absorción de agua of 0.2 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.18 g/cm³ Show Material materials with Densidad of 1.18 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 65 % Show Material materials with Elongación of 65 % | ASTM D 638 | Type I, 50 mm/min | ||
Elongation at yield | 23.0 °C | 4.1 % Show Material materials with Elongation at yield of 4.1 % | ASTM D 638 | Type I, 50 mm/min | ||
Flexural yield strength | 23.0 °C | 94 MPa Show Material materials with Flexural yield strength of 94 MPa | ISO 178 | 2 mm/min | ||
Impact strength, Izod notched, ASTM | -30.0 °C | 100 J/m Show Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D 256 | ||
23.0 °C | 475 J/m Show Material materials with Impact strength, Izod notched, ASTM of 475 J/m | ASTM D 256 | |||
Límite elástico | 23.0 °C | 63 MPa Show Material materials with Límite elástico of 63 MPa | ASTM D 638 | Type I, 50 mm/min | ||
Módulo de flexión | 23.0 °C | 2.44 GPa Show Material materials with Módulo de flexión of 2.44 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.76 GPa Show Material materials with Módulo elástico of 2.76 GPa | ASTM D 638 | 5 mm/min | ||
Resistencia a la tracción | 23.0 °C | 47 MPa Show Material materials with Resistencia a la tracción of 47 MPa | ASTM D 638 | Type I, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA | ||
23.0 °C | 33 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 33 kJ/m² | ISO 179/1eA | |||
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 12 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180/1A | ||
23.0 °C | 25 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 25 kJ/m² | ISO 180/1A | |||
Resistencia al choque, ensayo Charpy no entallado | No Break @ 23,-30°C | ISO 179/1eU | ||||
Resistencia al choque, ensayo Izod no entallado | No Break @ 23,-30°C| ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 98 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 98 °C | ISO 75/Bf | 0.45 MPa | |||
Relative temperature index, electrical | 85 °C Show Material materials with Relative temperature index, electrical of 85 °C | UL 746B | |||
Relative temperature index, mechanical impact | 85 °C Show Material materials with Relative temperature index, mechanical impact of 85 °C | UL 746B | |||
Relative temperature index, mechanical strength | 85 °C Show Material materials with Relative temperature index, mechanical strength of 85 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 106 °C Show Material materials with Temperatura de reblandecimiento Vicat of 106 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Compliant, 94V-0 Flame Class Rating | 1.5mm | UL 94 by SABIC-IP |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.9 [-] Show Material materials with Constante dieléctrica of 2.9 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 7E-3 [-] Show Material materials with Factor de disipación of 7E-3 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 31 kV/mm Show Material materials with Rigidez dieléctrica of 31 kV/mm | IEC 60243-1 | in oil, 1.6 mm |
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Material materials with Índice de seguimiento comparativo of 0 V | UL 746A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción of 0.4 - 0.6 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 23 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 23 cm³/10min | ISO 1133 | 260°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | ATM/Ticket Machine,Coffee Maker/Espresso Machine,Dishwasher,Displays,Electronic Components,Enclosures,Freezer,Medical Device,Non-LED Lighting,Refrigerator | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-300°C, Nozzle Temperature: 250-300°C, Front - Zone 3 Temperature: 250-300°C, Middle - Zone 2 Temperature: 240-290°C, Rear - Zone 1 Temperature: 230-280°C, Hopper Temperature: 60-80°C, Mold Temperature: 60-85°C, Vent Depth: 0.03-0.075mm |