General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.19 g/cm³ Show Material materials with Densidad of 1.19 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 100 % Show Material materials with Elongación of 100 % | ASTM D 638 | Type I, 50 mm/min |
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 93 MPa Show Material materials with Flexural yield strength of 93 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 587 J/m Show Material materials with Impact strength, Izod notched, ASTM of 587 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 62 MPa Show Material materials with Límite elástico of 62 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.5 GPa Show Material materials with Módulo de flexión of 2.5 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.96 GPa Show Material materials with Módulo elástico of 2.96 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la tracción | 23.0 °C | 59 MPa Show Material materials with Resistencia a la tracción of 59 MPa | ASTM D 638 | Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 40 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 40 kJ/m² | ISO 180/1A |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.38E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.38E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.46E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 8.46E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 85 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 85 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Relative temperature index, electrical | 60 °C Show Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 96 °C Show Material materials with Temperatura de reblandecimiento Vicat of 96 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating | 1.19mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.7 [-] Show Material materials with Constante dieléctrica of 2.7 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 8.6E-3 [-] Show Material materials with Factor de disipación of 8.6E-3 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 17 kV/mm Show Material materials with Rigidez dieléctrica of 17 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 - 0.5 % Show Material materials with Contracción of 0.3 - 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 18 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 18 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Velocidad de flujo del volumen derretido | 16 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 16 cm³/10min | ISO 1133 | 260°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management,Data Transfer,Displays,Document Handling,Enclosure/Housing/Cover,Enclosures,Exterior Trim,Individual Equiptment,Medical Device,Monitoring and Imaging,Non-LED Lighting,Personal Computing,Wireless Communications | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.04%, Melt Temperature: 245-275°C, Nozzle Temperature: 245-275°C, Front - Zone 3 Temperature: 245-275°C, Middle - Zone 2 Temperature: 220-265°C, Rear - Zone 1 Temperature: 220-255°C, Mold Temperature: 60-80°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 30-80%, Vent Depth: 0.038-0.076mm |