General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Material materials with Absorción de agua of 0.15 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.19 g/cm³ Show Material materials with Densidad of 1.19 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongation at yield | 23.0 °C | 7 % Show Material materials with Elongation at yield of 7 % | ISO 527 | 50 mm/min | ||
Flexural yield strength | 23.0 °C | 95 MPa Show Material materials with Flexural yield strength of 95 MPa | ISO 178 | 2 mm/min | ||
Límite elástico | 23.0 °C | 65 MPa Show Material materials with Límite elástico of 65 MPa | ISO 527 | 50 mm/min | ||
Módulo de flexión | 23.0 °C | 2.3 GPa Show Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.35 GPa Show Material materials with Módulo elástico of 2.35 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la tracción | 23.0 °C | 70 MPa Show Material materials with Resistencia a la tracción of 70 MPa | ISO 527 | 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 50 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 50 kJ/m² | ISO 179/1eA | ||
23.0 °C | 70 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 70 kJ/m² | ISO 179/1eA | |||
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 55 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 55 kJ/m² | ISO 180/1A | ||
23.0 °C | 75 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 75 kJ/m² | ISO 180/1A | |||
Resistencia al choque, ensayo Charpy no entallado | No Break @ 23,-30°C | ISO 179/1eU | ||||
Resistencia al choque, ensayo Izod no entallado | No Break @ 23,-30°C| ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | ISO 11359-2 | -23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 1.80 MPa | 130 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 130 °C | ISO 75/Af | 1.8 MPa | |||
Temperatura de reblandecimiento Vicat | 150 °C Show Material materials with Temperatura de reblandecimiento Vicat of 150 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating 2nd value | 3mm | UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 11 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 11 cm³/10min | ISO 1133 | 300°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Semiconductor Materials,Bottles,Building Element,Building/Construction Sheet,Cladding/Roof,LED Lighting,Small Appliance | |
Processing methods | Drying Temperature: 120°C, Drying Time: 2-4hrs, Barrel - Zone 1 Temperature: 240-270°C, Barrel - Zone 2 Temperature: 240-270°C, Barrel - Zone 3 Temperature: 240-270°C, Hopper Temperature: 100-120°C, Adapter Temperature: 220-260°C, Die Temperature: 220-280°C, Melt Temperature: 220-280°C |