General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.03 g/cm³ Show Material materials with Densidad of 1.03 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 32 % Show Material materials with Elongación of 32 % | ASTM D 638 | Type I, 5 mm/min |
Elongation at yield | 23.0 °C | 3.1 % Show Material materials with Elongation at yield of 3.1 % | ASTM D 638 | Type I, 5 mm/min |
Flexural yield strength | 23.0 °C | 60 MPa Show Material materials with Flexural yield strength of 60 MPa | ISO 178 | 2 mm/min |
Hardness, Rockwell R | 23.0 °C | 102 [-] Show Material materials with Hardness, Rockwell R of 102 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | -30.0 °C | 299 J/m Show Material materials with Impact strength, Izod notched, ASTM of 299 J/m | ASTM D 256 |
23.0 °C | 432 J/m Show Material materials with Impact strength, Izod notched, ASTM of 432 J/m | ASTM D 256 | |
Límite elástico | 23.0 °C | 39 MPa Show Material materials with Límite elástico of 39 MPa | ASTM D 638 | Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 2 GPa Show Material materials with Módulo de flexión of 2 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.08 GPa Show Material materials with Módulo elástico of 2.08 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 30 MPa Show Material materials with Resistencia a la tracción of 30 MPa | ASTM D 638 | Type I, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 37 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 37 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 23 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 23 kJ/m² | ISO 180/1A |
23.0 °C | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 35 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.01E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.01E-4 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.04E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1.04E-4 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 76 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 76 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Relative temperature index, electrical | 60 °C Show Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Temperatura de fusión | 215 - 230 °C Show Material materials with Temperatura de fusión of 215 - 230 °C | ||||
Temperatura de reblandecimiento Vicat | 106 °C Show Material materials with Temperatura de reblandecimiento Vicat of 106 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating | 1.5mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Material materials with Índice de seguimiento comparativo of 0 V | UL 746A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.6 - 0.8 % Show Material materials with Contracción of 0.6 - 0.8 % | SABIC method | 3.2 mm |
Melt viscosity | 23.0 °C | 1550 Pa·s Show Material materials with Melt viscosity of 1550 Pa·s | ASTM D 3825 | 240°C, 100 sec⁻¹ |
Velocidad de flujo de la masa derretida | 4 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 4 g/10min | ISO 1133 | 220°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Building/Construction Sheet,Enclosure/Housing/Cover,EV Infrastructure,Freezer,Heavy Vehicles,Refrigerator,Toy,Travel Suitcase | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 4-5hrs, Drying Time (Cumulative): 24hrs, Maximum Moisture Content: 0.02%, Barrel - Zone 1 Temperature: 205-225°C, Barrel - Zone 2 Temperature: 205-225°C, Barrel - Zone 3 Temperature: 205-225°C, Barrel - Zone 4 Temperature: 205-225°C, Adapter - Zone 5 Temperature: 210-230°C, Head - Zone 6 - Top Temperature: 215-230°C, Head - Zone 7 - Bottom Temperature: 215-230°C, Screw Speed: 20-60rpm, Extruder Feed Zone Temperature: 60-75°C, Mold Temperature: 40-80°C, Die Temperature: 215-235°C, Drying Temperature: 80-95°C, Drying Time: 4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 215-260°C, Barrel - Zone 1 Temperature: 170-200°C, Barrel - Zone 2 Temperature: 180-220°C, Barrel - Zone 3 Temperature: 190-225°C, Barrel - Zone 4 Temperature: 200-240°C, Adapter Temperature: 205-250°C, Die Temperature: 205-250°C, Roll Stack Temp - Top: 90-95°C, Roll Stack Temp - Middle: 95-105°C, Roll Stack Temp - Bottom: 100-105°C |