Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
SABIC® HDPE F00952 resin is a high molecular weight High Density Polyethylene copolymer which has been designed specifically for blown film extrusion. It has broad molecular distribution and high density combine succesfully to give excellent extrudability with high film strength and rigidity. The material contains anti oxidant. ApplicationSABIC® HDPE F00952 resin isrecommended for blown film extrusion. This product is suggested for the manufacture of high strength grocery sacks, shopping bags and high quality thin films for multi wall sack liners and replacement for thin paper products. Films of this poduct are readily treated and printed to give high quality graphics.Processing conditionsSABIC® HDPE F00952 can be extruded on conventional HMW-HDPE equipment at melt temperatures between 200 and 235 °C.Film propertiesFilm properties have been measured at 15 µm blown film with a BUR = 4.
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyethylene Wax: Uses and Properties
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationGeneral
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.95 g/cm³ Show Material materials with Densidad of 0.95 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Resistencia a desgarros | 23.0 °C | 117.6 kN/m Show Material materials with Resistencia a desgarros of 117.6 kN/m | ASTM D1922 |
Resistencia a desgarros transversal | 23.0 °C | 588 kN/m Show Material materials with Resistencia a desgarros transversal of 588 kN/m | ASTM D1922 |
Technological properties
Property | ||
---|---|---|
Application areas | Grocery sacks, shopping bags, thin films for multi wall sack liners, replacement for thin paper products. |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.