General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.03 g/cm³ Show Material materials with Densidad of 1.03 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 31.6 % Show Material materials with Elongación of 31.6 % | ASTM D 638 | Type I, 5 mm/min |
Elongation at yield | 23.0 °C | 3.1 % Show Material materials with Elongation at yield of 3.1 % | ASTM D 638 | Type I, 5 mm/min |
Flexural yield strength | 23.0 °C | 66 MPa Show Material materials with Flexural yield strength of 66 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | -30.0 °C | 299 J/m Show Material materials with Impact strength, Izod notched, ASTM of 299 J/m | ASTM D 256 |
23.0 °C | 432 J/m Show Material materials with Impact strength, Izod notched, ASTM of 432 J/m | ASTM D 256 | |
Límite elástico | 23.0 °C | 39 MPa Show Material materials with Límite elástico of 39 MPa | ASTM D 638 | Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 2.16 GPa Show Material materials with Módulo de flexión of 2.16 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 2.08 GPa Show Material materials with Módulo elástico of 2.08 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 30 MPa Show Material materials with Resistencia a la tracción of 30 MPa | ASTM D 638 | Type I, 5 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.01E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.01E-4 1/K | ASTM E 831 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.04E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1.04E-4 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature, 1.80 MPa | 80 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 80 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Temperatura de fusión | 215 - 230 °C Show Material materials with Temperatura de fusión of 215 - 230 °C | ||
Temperatura de reblandecimiento Vicat | 106 °C Show Material materials with Temperatura de reblandecimiento Vicat of 106 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.6 - 0.8 % Show Material materials with Contracción of 0.6 - 0.8 % | SABIC method | 3.2 mm |
Melt viscosity | 23.0 °C | 1400 Pa·s Show Material materials with Melt viscosity of 1400 Pa·s | ASTM D 3825 | 240°C, 100 sec⁻¹ |
Velocidad de flujo del volumen derretido | 4 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 4 cm³/10min | ISO 1133 | 220°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Building/Construction Sheet,Data Management,Heavy Vehicles,Monitoring and Imaging | |
Processing methods | Drying Temperature: 80-90°C, Drying Time: 4-5hrs, Drying Time (Cumulative): 24hrs, Maximum Moisture Content: 0.02%, Barrel - Zone 1 Temperature: 205-225°C, Barrel - Zone 2 Temperature: 205-225°C, Barrel - Zone 3 Temperature: 205-225°C, Barrel - Zone 4 Temperature: 205-225°C, Adapter - Zone 5 Temperature: 210-230°C, Head - Zone 6 - Top Temperature: 215-230°C, Head - Zone 7 - Bottom Temperature: 215-230°C, Screw Speed: 20-60rpm, Extruder Feed Zone Temperature: 60-75°C, Mold Temperature: 40-80°C, Die Temperature: 215-235°C, Drying Temperature: 80-95°C, Drying Time: 4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 215-260°C, Barrel - Zone 1 Temperature: 170-200°C, Barrel - Zone 2 Temperature: 180-220°C, Barrel - Zone 3 Temperature: 190-225°C, Barrel - Zone 4 Temperature: 200-240°C, Adapter Temperature: 205-250°C, Die Temperature: 205-250°C, Roll Stack Temp - Top: 90-95°C, Roll Stack Temp - Middle: 95-105°C, Roll Stack Temp - Bottom: 100-105°C |