General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Material materials with Absorción de agua of 0.1 % | ASTM D 570 | 24 Hours |
Absorción de agua, equilibrio | 100.0 °C | 0.58 % Show Material materials with Absorción de agua, equilibrio of 0.58 % | ASTM D 570 | ASTM D 570 |
Densidad | 23.0 °C | 1.2 g/cm³ Show Material materials with Densidad of 1.2 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 120 % Show Material materials with Elongación of 120 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 93 MPa Show Material materials with Flexural yield strength of 93 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | 23.0 °C | 640 J/m Show Material materials with Impact strength, Izod notched, ASTM of 640 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 62 MPa Show Material materials with Límite elástico of 62 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 65 MPa Show Material materials with Resistencia a la tracción of 65 MPa | ASTM D 638 | Type I, 50 mm/min |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 126 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Relative temperature index, electrical | 130 °C Show Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 130 °C Show Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |
Relative temperature index, mechanical strength | 130 °C Show Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |
Inflamabilidad | UL Recognized, 94V-2 Flame Class Rating | 1.09mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Material materials with Índice de seguimiento comparativo of 2 V | UL 746A |
Óptico
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 25 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 25 g/10min | ASTM D 1238 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Amusement Machine,ATM/Ticket Machine,Audio,Auto Aftermarket,Coffee Maker/Espresso Machine,Cooking Range,Data Management,Data Transfer,Dishwasher,Displays,Document Handling,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Food Processor,Forward Lighting,Fused Deposition Modeling (FDM),Heavy Vehicles,Industrial Material Handling,Infotainment/Telematic,Lab Ware and Clinical Diagnostics,Laundry Dryer,Medical Device,Meter Gas,Monitoring and Imaging,Non-LED Lighting,Overhead,Personal Care,Personal Computing,Pharmaceutical Packaging & Drug Delivery,Photo/Video Camera,Power Manangement,Rear/Signal Lighting,Recreational Vehicle,Respiratory,Small Appliance,Surgical Devices,Vacuum Cleaner,Vending Machine,Washing Machine,Watch/Jewelry,Wearables,Wireless Communications,Wiring Devices | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 270-295°C, Nozzle Temperature: 265-290°C, Front - Zone 3 Temperature: 270-295°C, Middle - Zone 2 Temperature: 260-280°C, Rear - Zone 1 Temperature: 250-270°C, Mold Temperature: 70-95°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm |