General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.92 g/cm³ Show Material materials with Densidad of 0.92 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 43 [-] Show Material materials with Dureza Shore D of 43 [-] | ASTM D2240 |
Elongación | 23.0 °C | 80 % Show Material materials with Elongación of 80 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 490 J/m Show Material materials with Impact strength, Izod notched, ASTM of 490 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 9 MPa Show Material materials with Límite elástico of 9 MPa | ASTM D638 |
Resistencia a la tracción | 23.0 °C | 10.5 MPa Show Material materials with Resistencia a la tracción of 10.5 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de reblandecimiento Vicat | 89 °C Show Material materials with Temperatura de reblandecimiento Vicat of 89 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 7 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 7 g/10min | ASTM D1238 | 190°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Caps & closures,Masterbatch |