General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.2 % Show Material materials with Absorción de agua of 0.2 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.15 g/cm³ Show Material materials with Densidad of 1.15 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 125 % Show Material materials with Elongación of 125 % | ISO 527 | 5 mm/min |
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ISO 527 | 50 mm/min |
Flexural yield strength | 23.0 °C | 85 MPa Show Material materials with Flexural yield strength of 85 MPa | ISO 178 | 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 106 MPa Show Material materials with Hardness, Ball Indentation of 106 MPa | ISO 2039-1 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Material materials with Hardness, Rockwell R of 120 [-] | ISO 2039-2 |
Límite elástico | 23.0 °C | 62 MPa Show Material materials with Límite elástico of 62 MPa | ISO 527 | 50 mm/min |
Módulo de flexión | 23.0 °C | 2.4 GPa Show Material materials with Módulo de flexión of 2.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.5 GPa Show Material materials with Módulo elástico of 2.5 GPa | ISO 527 | 1 mm/min |
Resistencia a la tracción | 23.0 °C | 62 MPa Show Material materials with Resistencia a la tracción of 62 MPa | ISO 527 | 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 12 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | ISO 179/1eA |
23.0 °C | 60 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 60 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 15 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 15 kJ/m² | ISO 180/1A |
23.0 °C | 45 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 45 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 1.80 MPa | 112 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 112 °C | ISO 75/Ae | 1.8 MPa | |||
Temperatura de reblandecimiento Vicat | 132 °C Show Material materials with Temperatura de reblandecimiento Vicat of 132 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Compliant, 94HB Flame Class Rating | 1.6mm | UL 94 by SABIC-IP |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.8 [-] Show Material materials with Constante dieléctrica of 2.8 [-] | IEC 60250 | at 1 MHz |
Factor de disipación | 23.0 °C | 0.01 [-] Show Material materials with Factor de disipación of 0.01 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 17 kV/mm Show Material materials with Rigidez dieléctrica of 17 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 225 V Show Material materials with Índice de seguimiento comparativo of 225 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción of 0.4 - 0.6 % | SABIC method |
Velocidad de flujo del volumen derretido | 17 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 17 cm³/10min | ISO 1133 | 260°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Cladding,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Exterior Trim,Exterior,Forward Lighting,Front Grille,Interior,Lighting,Meter Gas,Non-LED Lighting,Overhead,Personal Computing,Rear/Signal Lighting,Recreational Vehicle,Spoiler,Vacuum Cleaner,Wireless Communications,Wiring Devices | |
Processing methods | Drying Temperature: 100-110°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 260-290°C, Nozzle Temperature: 240-280°C, Front - Zone 3 Temperature: 250-290°C, Middle - Zone 2 Temperature: 250-290°C, Rear - Zone 1 Temperature: 230-260°C, Hopper Temperature: 60-80°C, Mold Temperature: 60-90°C |