General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.16 g/cm³ Show Material materials with Densidad of 1.16 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 77 [-] Show Material materials with Dureza Shore D of 77 [-] | ISO 868 |
Elongación | 23.0 °C | 160 % Show Material materials with Elongación of 160 % | ASTM D 638 | Type I, 5 mm/min |
Elongation at yield | 23.0 °C | 5 % Show Material materials with Elongation at yield of 5 % | ASTM D 638 | Type I, 5 mm/min |
Flexural yield strength | 23.0 °C | 80 MPa Show Material materials with Flexural yield strength of 80 MPa | ISO 178 | 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 63 MPa Show Material materials with Hardness, Ball Indentation of 63 MPa | ISO 2039-1 |
Hardness, Rockwell L | 23.0 °C | 57 [-] Show Material materials with Hardness, Rockwell L of 57 [-] | ISO 2039-2 |
Impact strength, Izod notched, ASTM | -30.0 °C | 140 J/m Show Material materials with Impact strength, Izod notched, ASTM of 140 J/m | ASTM D 256 |
23.0 °C | 450 J/m Show Material materials with Impact strength, Izod notched, ASTM of 450 J/m | ASTM D 256 | |
Límite elástico | 23.0 °C | 50 MPa Show Material materials with Límite elástico of 50 MPa | ASTM D 638 | Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 2.1 GPa Show Material materials with Módulo de flexión of 2.1 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.16 GPa Show Material materials with Módulo elástico of 2.16 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 58 MPa Show Material materials with Resistencia a la tracción of 58 MPa | ASTM D 638 | Type I, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 17 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 17 kJ/m² | ISO 179/1eA |
23.0 °C | 45 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 45 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 14 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 14 kJ/m² | ISO 180/1A |
23.0 °C | 45 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 45 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Material materials with Surface resistivity of 1.00E+13 Ω/sq | IEC 60093 | ROA |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 8 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 8 g/10min | ISO 1133 | 220°C/10.0 kg |
Velocidad de flujo del volumen derretido | 29 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 29 cm³/10min | ISO 1133 | 260°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Overhead | |
Processing methods | Drying Temperature: 85-95°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.04%, Melt Temperature: 255-270°C, Nozzle Temperature: 235-255°C, Front - Zone 3 Temperature: 245-260°C, Middle - Zone 2 Temperature: 235-255°C, Rear - Zone 1 Temperature: 230-250°C, Mold Temperature: 60-85°C, Back Pressure: 0.3-1MPa, Screw Speed: 30-80rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.038-0.076mm |