Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
CYCOLAC™ Resin INP338
SABIC INP338 is an ultra high rubber ABS impact modifier resin, and is based on polybutadiene rubber. Offers superior impact efficiency, especially at low temperatures. Reduces notch sensitivity when alloyed with engineering polymers. Disperses easily. Provides abrasion and chemical resistance to polymers. Provides toughness to PVC sheet, profile, electrical conduit and injection molded applications. Increases the impact strength of recycle PVC and other recyclates. Can be blended with polyurethanes and other polymers for improved performance and economics. Can be used to improve the impact performance of PC, polyesters, and CPVC. Powder. FDA compliant (part use must be at room temperature or below).
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationGeneral
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.95 g/cm³ Show Material materials with Densidad of 0.95 g/cm³ | ASTM D 792 |
Densidad aparente | 23.0 °C | 0.25 g/cm³ Show Material materials with Densidad aparente of 0.25 g/cm³ | ASTM D 1895 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 40 [-] Show Material materials with Dureza Shore D of 40 [-] | ASTM D 2240 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 5.7 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 5.7 g/10min | ASTM D 1238 | 200°C/3.8 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Semiconductor Materials |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.