General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.07 g/cm³ Show Material materials with Densidad of 1.07 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Flexural yield strength | 23.0 °C | 38 MPa Show Material materials with Flexural yield strength of 38 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 18 J/m Show Material materials with Impact strength, Izod notched, ASTM of 18 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 3.4 GPa Show Material materials with Módulo de flexión of 3.4 GPa | ISO 178 | 2 mm/min |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 1 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 1 kJ/m² | ISO 180/1A |
23.0 °C | 2 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 2 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 86 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 86 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed |
Temperatura de reblandecimiento Vicat | 102 °C Show Material materials with Temperatura de reblandecimiento Vicat of 102 °C | ISO 306 | Rate B/120 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 0 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 0 g/10min | ISO 1133 | 220°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures |