General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Material materials with Absorción de agua of 0.15 % | ISO 62 | 23°C, 50% RH |
Absorción de agua, equilibrio | 23.0 °C | 0.35 % Show Material materials with Absorción de agua, equilibrio of 0.35 % | ASTM D 570 |
Densidad | 23.0 °C | 1.19 g/cm³ Show Material materials with Densidad of 1.19 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 135 % Show Material materials with Elongación of 135 % | ASTM D 638 | Type I, 50 mm/min |
Elongation at yield | 23.0 °C | 7 % Show Material materials with Elongation at yield of 7 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 90 MPa Show Material materials with Flexural yield strength of 90 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | -30.0 °C | 139 J/m Show Material materials with Impact strength, Izod notched, ASTM of 139 J/m | ASTM D 256 |
23.0 °C | 850 J/m Show Material materials with Impact strength, Izod notched, ASTM of 850 J/m | ASTM D 256 | |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 3204 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m | ASTM D 4812 |
Límite elástico | 23.0 °C | 63 MPa Show Material materials with Límite elástico of 63 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.31 GPa Show Material materials with Módulo elástico of 2.31 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 68 MPa Show Material materials with Resistencia a la tracción of 68 MPa | ASTM D 638 | Type I, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 95 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 95 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A |
23.0 °C | 65 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 65 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 6E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 6E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 6E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Heat deflection temperature, 1.80 MPa | 132 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 132 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed | |
Temperatura de reblandecimiento Vicat | 154 °C Show Material materials with Temperatura de reblandecimiento Vicat of 154 °C | ASTM D 1525 | Rate B/50 |
Óptico
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 7 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 7 g/10min | ASTM D 1238 | 300°C/1.2 kg | |
Velocidad de flujo del volumen derretido | 6 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 6 cm³/10min | ISO 1133 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Sunglasses | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 310-330°C, Nozzle Temperature: 305-325°C, Front - Zone 3 Temperature: 310-330°C, Middle - Zone 2 Temperature: 300-320°C, Rear - Zone 1 Temperature: 290-310°C, Mold Temperature: 80-115°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm |