General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Material materials with Absorción de agua of 0.15 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.34 g/cm³ Show Material materials with Densidad of 1.34 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 120 % Show Material materials with Elongación of 120 % | ASTM D 638 | Type I, 50 mm/min |
Elongation at yield | 23.0 °C | 6 % Show Material materials with Elongation at yield of 6 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 98 MPa Show Material materials with Flexural yield strength of 98 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | -30.0 °C | 165 J/m Show Material materials with Impact strength, Izod notched, ASTM of 165 J/m | ASTM D 256 |
23.0 °C | 648 J/m Show Material materials with Impact strength, Izod notched, ASTM of 648 J/m | ASTM D 256 | |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2130 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 2130 J/m | ASTM D 4812 |
Límite elástico | 23.0 °C | 60 MPa Show Material materials with Límite elástico of 60 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.5 GPa Show Material materials with Módulo de flexión of 2.5 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 70 MPa Show Material materials with Resistencia a la flexión of 70 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 61 MPa Show Material materials with Resistencia a la tracción of 61 MPa | ASTM D 638 | Type I, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 12 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | ISO 179/1eA |
23.0 °C | 67 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 67 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30.0 °C | 140 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 140 kJ/m² | ISO 179/1eU |
23.0 °C | 140 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 140 kJ/m² | ISO 179/1eU | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 13 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 13 kJ/m² | ISO 180/1A |
23.0 °C | 52 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 52 kJ/m² | ISO 180/1A | |
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 160 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 160 kJ/m² | ISO 180/1U |
23.0 °C | 170 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 170 kJ/m² | ISO 180/1U | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 6.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 6.3E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 124 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Temperatura de reblandecimiento Vicat | 142 °C Show Material materials with Temperatura de reblandecimiento Vicat of 142 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-2 Flame Class Rating | 1.5mm | UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 17 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 17 g/10min | ASTM D 1238 | 300°C/1.2 kg | |
Velocidad de flujo del volumen derretido | 16 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 16 cm³/10min | ISO 1133 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Displays,Enclosures,Forward Lighting,Rear/Signal Lighting | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 280-305°C, Nozzle Temperature: 275-300°C, Front - Zone 3 Temperature: 280-305°C, Middle - Zone 2 Temperature: 270-295°C, Rear - Zone 1 Temperature: 260-280°C, Mold Temperature: 70-95°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm |