General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.04 g/cm³ Show Material materials with Densidad of 1.04 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 26 % Show Material materials with Elongación of 26 % | ASTM D 638 | Type I, 5 mm/min |
Elongation at yield | 23.0 °C | 2.4 % Show Material materials with Elongation at yield of 2.4 % | ASTM D 638 | Type I, 5 mm/min |
Flexural yield strength | 23.0 °C | 61 MPa Show Material materials with Flexural yield strength of 61 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 455 J/m Show Material materials with Impact strength, Izod notched, ASTM of 455 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 39 MPa Show Material materials with Límite elástico of 39 MPa | ASTM D 638 | Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 1.99 GPa Show Material materials with Módulo de flexión of 1.99 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2 GPa Show Material materials with Módulo elástico of 2 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 31 MPa Show Material materials with Resistencia a la tracción of 31 MPa | ASTM D 638 | Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 12 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180/1A |
23.0 °C | 37 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 37 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 9.54E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9.54E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 9.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 9.36E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 79 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 79 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Relative temperature index, electrical | 60 °C Show Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 99 °C Show Material materials with Temperatura de reblandecimiento Vicat of 99 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating | 1.5mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Material materials with Índice de seguimiento comparativo of 0 V | UL 746A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.8 % Show Material materials with Contracción of 0.5 - 0.8 % | SABIC method | 3.2 mm |
Melt viscosity | 23.0 °C | 280 Pa·s Show Material materials with Melt viscosity of 280 Pa·s | ASTM D 3825 | 240°C, 1000 sec⁻¹ |
Velocidad de flujo de la masa derretida | 8 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 8 g/10min | ISO 1133 | 220°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Body Protection,Building Accessory,Document Handling,Enclosure/Housing/Cover,Head Protection,Lab Ware and Clinical Diagnostics,Lawn/Garden,Medical Device,Surgical Devices,Water Treatment/Filtration,Irrigation | |
Processing methods | Drying Temperature: 90-95°C, Drying Time: 2-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.1%, Melt Temperature: 230-275°C, Nozzle Temperature: 230-275°C, Front - Zone 3 Temperature: 225-240°C, Middle - Zone 2 Temperature: 210-220°C, Rear - Zone 1 Temperature: 190-200°C, Mold Temperature: 50-65°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 30-60rpm, Shot to Cylinder Size: 50-70%, Vent Depth: 0.038-0.051mm |