General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.05 g/cm³ Show Material materials with Densidad of 1.05 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 15.8 % Show Material materials with Elongación of 15.8 % | ISO 527 | 5 mm/min |
Elongation at yield | 23.0 °C | 2 % Show Material materials with Elongation at yield of 2 % | ISO 527 | 5 mm/min |
Flexural yield strength | 23.0 °C | 73 MPa Show Material materials with Flexural yield strength of 73 MPa | ISO 178 | 2 mm/min |
Límite elástico | 23.0 °C | 48 MPa Show Material materials with Límite elástico of 48 MPa | ISO 527 | 5 mm/min |
Módulo de flexión | 23.0 °C | 2.47 GPa Show Material materials with Módulo de flexión of 2.47 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.76 GPa Show Material materials with Módulo elástico of 2.76 GPa | ISO 527 | 1 mm/min |
Resistencia a la tracción | 23.0 °C | 39 MPa Show Material materials with Resistencia a la tracción of 39 MPa | ISO 527 | 5 mm/min |
Resistencia al choque, ensayo Izod entallado | -40.0 °C | 6 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A |
-30.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | |
23.0 °C | 23 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 23 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 6E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 6E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 6E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Heat deflection temperature, 1.80 MPa | 82 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ISO 75/Af | 1.8 MPa | |
Temperatura de reblandecimiento Vicat | 98 °C Show Material materials with Temperatura de reblandecimiento Vicat of 98 °C | ISO 306 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción of 0.4 - 0.6 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 20.6 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 20.6 g/10min | ASTM D 1238 | 220°C/10 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors,Applique,Auto Aftermarket,Body Protection,Cladding,Cluster,Console,Data Management,Dishwasher,Document Handling,Door Handle,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Exterior Mirror,Exterior Rail Components,Exterior Trim,Exterior,Fixture Bath/Shower,Food Processor,Food Transportation,Front Grille,Heavy Vehicles,Hygiene/Personal Care,Laundry Dryer,Lawn/Garden,LED Lighting,Lighting,Long Distance Coach,Medical Device,Medical Facility Infrastructure,Modular Panel,Monitoring and Imaging,Motorcycle,Neighborhood Electric Vehicle,Non-LED Lighting,Personal Water Craft,Pharmaceutical Packaging & Drug Delivery,Plumbing,Power Manangement,Rail Cabin Interiors,Rail,Rear/Signal Lighting,Recreational Vehicle,Refrigerator,Renal and Blood Handling,Respiratory,Seat,Skid Plate,Small Appliance,Surgical Devices,Trim,Underbody Shield,Washing Machine,Watch/Jewelry,Wheel Cover,Wireless Communications,Wiring Devices,Irrigation | |
Processing methods | Drying Temperature: 80-95°C, Drying Time: 2-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.05%, Melt Temperature: 255-280°C, Nozzle Temperature: 255-280°C, Front - Zone 3 Temperature: 250-270°C, Middle - Zone 2 Temperature: 230-245°C, Rear - Zone 1 Temperature: 215-230°C, Mold Temperature: 40-80°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 30-60rpm, Shot to Cylinder Size: 50-70%, Vent Depth: 0.038-0.051mm |