General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.04 g/cm³ Show Material materials with Densidad of 1.04 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 24 % Show Material materials with Elongación of 24 % | ASTM D 638 | Type I, 5 mm/min |
Elongation at yield | 23.0 °C | 2 % Show Material materials with Elongation at yield of 2 % | ASTM D 638 | Type I, 5 mm/min |
Flexural yield strength | 23.0 °C | 70 MPa Show Material materials with Flexural yield strength of 70 MPa | ISO 178 | 2 mm/min |
Hardness, Rockwell R | 23.0 °C | 112 [-] Show Material materials with Hardness, Rockwell R of 112 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 320 J/m Show Material materials with Impact strength, Izod notched, ASTM of 320 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 44 MPa Show Material materials with Límite elástico of 44 MPa | ASTM D 638 | Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 2.2 GPa Show Material materials with Módulo de flexión of 2.2 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.27 GPa Show Material materials with Módulo elástico of 2.27 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la tracción | 23.0 °C | 33 MPa Show Material materials with Resistencia a la tracción of 33 MPa | ASTM D 638 | Type I, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 9 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | ISO 179/1eA |
23.0 °C | 26 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 26 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A |
23.0 °C | 22 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 22 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8.82E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8.82E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.82E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 8.82E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 80 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 80 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Relative temperature index, electrical | 60 °C Show Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 99 °C Show Material materials with Temperatura de reblandecimiento Vicat of 99 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating | 1.5mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Material materials with Índice de seguimiento comparativo of 0 V | UL 746A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.8 % Show Material materials with Contracción of 0.5 - 0.8 % | SABIC method | 3.2 mm |
Melt viscosity | 23.0 °C | 225 Pa·s Show Material materials with Melt viscosity of 225 Pa·s | ASTM D 3825 | 240°C, 1000 sec⁻¹ |
Velocidad de flujo de la masa derretida | 18 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 18 g/10min | ISO 1133 | 220°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors,Air Filtration,Amusement Machine,Animal Testing,Applique,Audio,Auto Aftermarket,Building Accessory,Building Element,Circuit Protection,Cluster,Coffee Maker/Espresso Machine,Commercial Storage/Cookware,Console,Data Management,Data Transfer,Dishwasher,Displays,Document Handling,Door Handle,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Exterior Mirror,Exterior Trim,Food Container,Food Transportation,Front Grille,Fused Deposition Modeling (FDM),Gas/Electric Oven,Head Protection,Heavy Vehicles,Industrial Material Handling,Interior,Lab Ware and Clinical Diagnostics,Laundry Dryer,Lawn/Garden,Medical Device,Medical Facility Infrastructure,Meter Water,Non-LED Lighting,Overhead,Personal Computing,Personal Water Craft,Pharmaceutical Manufacturing,Pharmaceutical Packaging & Drug Delivery,Power Manangement,Pump,Rear/Signal Lighting,Refrigerator,Respiratory,Security/Detection,Small Appliance,Storage/Table,Surgical Devices,Swimming Pool/Spa,Travel Suitcase,Vacuum Cleaner,Vending Machine,Washing Machine,Water Treatment/Filtration,Wearables,Wireless Communications,Wiring Devices | |
Processing methods | Drying Temperature: 80-95°C, Drying Time: 2-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.1%, Melt Temperature: 220-260°C, Nozzle Temperature: 220-260°C, Front - Zone 3 Temperature: 215-240°C, Middle - Zone 2 Temperature: 205-225°C, Rear - Zone 1 Temperature: 190-210°C, Mold Temperature: 50-70°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 30-60rpm, Shot to Cylinder Size: 50-70%, Vent Depth: 0.038-0.051mm |