General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.2 g/cm³ Show Material materials with Densidad of 1.2 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 135 % Show Material materials with Elongación of 135 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 96 MPa Show Material materials with Flexural yield strength of 96 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | 23.0 °C | 907 J/m Show Material materials with Impact strength, Izod notched, ASTM of 907 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 62 MPa Show Material materials with Límite elástico of 62 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.34 GPa Show Material materials with Módulo de flexión of 2.34 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 68 MPa Show Material materials with Resistencia a la tracción of 68 MPa | ASTM D 638 | Type I, 50 mm/min |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 132 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 132 °C | ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed |
Óptico
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción of 0.5 - 0.7 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 7.5 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 7.5 g/10min | ASTM D 1238 | 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components,Enclosures,Head Protection,Individual Equiptment,LED Lighting,Meter Water,Respiratory,Safety Glasses,Wireless Communications | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 310-330°C, Nozzle Temperature: 305-325°C, Front - Zone 3 Temperature: 310-330°C, Middle - Zone 2 Temperature: 300-320°C, Rear - Zone 1 Temperature: 290-310°C, Mold Temperature: 80-115°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm |