Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
HDPE P5616N is a multimodal high density polyethylene Natural grade specially developed for f non-pressure pipe applications. The material offers easy flow, higher stiffness, very good ESCR and sufficient impact strength.
Los datos sobre este material han sido proporcionados por Matmatch.
See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyethylene Wax: Uses and Properties
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationGeneral
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.96 g/cm³ Show Material materials with Densidad of 0.96 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 62 [-] Show Material materials with Dureza Shore D of 62 [-] | ASTM D2240 |
Elongation at yield | 23.0 °C | 8 % Show Material materials with Elongation at yield of 8 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 27 MPa Show Material materials with Límite elástico of 27 MPa | ISO 527-1/-2 |
Módulo elástico | 23.0 °C | 1.3 GPa Show Material materials with Módulo elástico of 1.3 GPa | ASTM D638 |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe/Fitting |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.