General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.94 g/cm³ Show Material materials with Densidad of 0.94 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 66 [-] Show Material materials with Dureza Shore D of 66 [-] | ISO 868 |
Módulo de flexión | 23.0 °C | 0.42 GPa Show Material materials with Módulo de flexión of 0.42 GPa | ASTM D790 A |
Resistencia a la flexión | 23.0 °C | 13 MPa Show Material materials with Resistencia a la flexión of 13 MPa | ASTM D790 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de reblandecimiento Vicat | 114 °C Show Material materials with Temperatura de reblandecimiento Vicat of 114 °C | ASTM D1525 |