General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.03 % Show Material materials with Absorción de agua of 0.03 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.44 g/cm³ Show Material materials with Densidad of 1.44 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Material materials with Elongación of 2 % | ASTM D 638 | Type I, 5 mm/min |
Elongation at yield | 23.0 °C | 2 % Show Material materials with Elongation at yield of 2 % | ASTM D 638 | Type I, 5 mm/min |
Flexural strain | 23.0 °C | 3 % Show Material materials with Flexural strain of 3 % | ISO 178 | 2 mm/min |
Flexural yield strength | 23.0 °C | 160 MPa Show Material materials with Flexural yield strength of 160 MPa | ISO 178 | 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 185 MPa Show Material materials with Hardness, Ball Indentation of 185 MPa | ISO 2039-1 |
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Material materials with Hardness, Rockwell R of 118 [-] | ISO 2039-2 |
Impact strength, Izod notched, ASTM | -30.0 °C | 80 J/m Show Material materials with Impact strength, Izod notched, ASTM of 80 J/m | ASTM D 256 |
23.0 °C | 80 J/m Show Material materials with Impact strength, Izod notched, ASTM of 80 J/m | ASTM D 256 | |
Impact strength, Izod unnotched, ASTM | -30.0 °C | 330 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 330 J/m | ASTM D 4812 |
23.0 °C | 350 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 350 J/m | ASTM D 4812 | |
Límite elástico | 23.0 °C | 105 MPa Show Material materials with Límite elástico of 105 MPa | ASTM D 638 | Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 5.6 GPa Show Material materials with Módulo de flexión of 5.6 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 6.8 GPa Show Material materials with Módulo elástico of 6.8 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 160 MPa Show Material materials with Resistencia a la flexión of 160 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 105 MPa Show Material materials with Resistencia a la tracción of 105 MPa | ASTM D 638 | Type I, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 9 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | ISO 179/2C |
23.0 °C | 9 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | ISO 179/2C | |
Resistencia al choque, ensayo Charpy no entallado | -30.0 °C | 25 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 25 kJ/m² | ISO 179/2C |
23.0 °C | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | ISO 179/2C | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A |
23.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 30 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 30 kJ/m² | ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 4E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 1E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1E-4 1/K | ISO 11359-2 | -40°C to 40°C |
Heat deflection temperature, 0.45 MPa | 223 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 223 °C | ISO 75/Bf | 0.45 MPa | |
Temperatura de reblandecimiento Vicat | 205 °C Show Material materials with Temperatura de reblandecimiento Vicat of 205 °C | ASTM D 1525 | Rate B/50 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Factor de disipación | 23.0 °C | 0.02 [-] Show Material materials with Factor de disipación of 0.02 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 18.6 kV/mm Show Material materials with Rigidez dieléctrica of 18.6 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 375 V Show Material materials with Índice de seguimiento comparativo of 375 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 - 0.7 % Show Material materials with Contracción of 0.3 - 0.7 % | SABIC method |
Contracción transversal | 23.0 °C | 0.4 - 1 % Show Material materials with Contracción transversal of 0.4 - 1 % | SABIC method |
Melt viscosity | 260.0 °C | 55 Pa·s Show Material materials with Melt viscosity of 55 Pa·s | ISO 11443 | ISO 11443 | 250°C, 1500 sec⁻¹ |
Velocidad de flujo del volumen derretido | 40 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 40 cm³/10min | ISO 1133 | 250°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components | |
Fillers | 20% Glass Fiber | |
Processing methods | Drying Temperature: 110-120°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-270°C, Nozzle Temperature: 240-260°C, Front - Zone 3 Temperature: 245-265°C, Middle - Zone 2 Temperature: 240-255°C, Rear - Zone 1 Temperature: 230-245°C, Hopper Temperature: 40-60°C, Mold Temperature: 40-100°C |