General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.07 % Show Material materials with Absorción de agua of 0.07 % | ASTM D 570 | 24 Hours |
Densidad | 23.0 °C | 1.42 g/cm³ Show Material materials with Densidad of 1.42 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Material materials with Elongación of 5 % | SABIC - Japan Method |
Impact strength, Izod notched, ASTM | 23.0 °C | 137 J/m Show Material materials with Impact strength, Izod notched, ASTM of 137 J/m | ASTM D 256 |
Límite elástico | 23.0 °C | 96 MPa Show Material materials with Límite elástico of 96 MPa | SABIC - Japan Method |
Módulo de flexión | 23.0 °C | 6.08 GPa Show Material materials with Módulo de flexión of 6.08 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 128 MPa Show Material materials with Resistencia a la flexión of 128 MPa | ASTM D 790 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 3E-5 1/K | TMA | -30°C to 30°C |
Heat deflection temperature, 1.80 MPa | 205 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3 [-] Show Material materials with Constante dieléctrica of 3 [-] | ASTM D 150 | at 50/60 Hz |
Volume resistivity | 23.0 °C | 1.00E+18 Ω·cm Show Material materials with Volume resistivity of 1.00E+18 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.6 - 0.8 % Show Material materials with Contracción of 0.6 - 0.8 % | SABIC method | 6.4 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Auto Aftermarket,Data Transfer,Electronic Components,Enclosures,EV Infrastructure | |
Fillers | 30% Glass Fiber |