General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.14 % Show Material materials with Absorción de agua of 0.14 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.35 g/cm³ Show Material materials with Densidad of 1.35 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 8 % Show Material materials with Elongación of 8 % | ISO 527 | 5 mm/min |
Elongation at yield | 23.0 °C | 3.2 % Show Material materials with Elongation at yield of 3.2 % | ISO 527 | 5 mm/min |
Flexural yield strength | 23.0 °C | 90 MPa Show Material materials with Flexural yield strength of 90 MPa | ISO 178 | 2 mm/min |
Límite elástico | 23.0 °C | 56 MPa Show Material materials with Límite elástico of 56 MPa | ISO 527 | 5 mm/min |
Módulo de flexión | 23.0 °C | 4.05 GPa Show Material materials with Módulo de flexión of 4.05 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 4.15 GPa Show Material materials with Módulo elástico of 4.15 GPa | ISO 527 | 1 mm/min |
Resistencia a la tracción | 23.0 °C | 50 MPa Show Material materials with Resistencia a la tracción of 50 MPa | ISO 527 | 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 6 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A |
23.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | |
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 80 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 80 kJ/m² | ISO 180/1U |
23.0 °C | 100 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 100 kJ/m² | ISO 180/1U | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 5.2E-5 1/K | ISO 11359-2 | -30°C to 80°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 7.2E-5 1/K | ISO 11359-2 | -30°C to 80°C |
Heat deflection temperature, 1.80 MPa | 110 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 110 °C | ISO 75/Af | 1.8 MPa | |
Temperatura de reblandecimiento Vicat | 140 °C Show Material materials with Temperatura de reblandecimiento Vicat of 140 °C | ISO 306 | Rate B/120 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo del volumen derretido | 15 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | ISO 1133 | 265°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Lawn/Garden,Spoiler | |
Fillers | Mineral Powder | |
Processing methods | Drying Temperature: 110-120°C, Drying Time: 4-6hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 265-275°C, Nozzle Temperature: 260-275°C, Front - Zone 3 Temperature: 260-280°C, Middle - Zone 2 Temperature: 250-275°C, Rear - Zone 1 Temperature: 240-270°C, Hopper Temperature: 60-80°C, Mold Temperature: 60-100°C |