General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 92 % Show Material materials with Elongación of 92 % | ASTM D 638 | Type I, 50 mm/min |
Elongation at yield | 23.0 °C | 6 % Show Material materials with Elongation at yield of 6 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 94 MPa Show Material materials with Flexural yield strength of 94 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched, ASTM | -30.0 °C | 200 J/m Show Material materials with Impact strength, Izod notched, ASTM of 200 J/m | ASTM D 256 |
23.0 °C | 854 J/m Show Material materials with Impact strength, Izod notched, ASTM of 854 J/m | ASTM D 256 | |
Límite elástico | 23.0 °C | 57 MPa Show Material materials with Límite elástico of 57 MPa | ASTM D 638 | Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2 GPa Show Material materials with Módulo de flexión of 2 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.37 GPa Show Material materials with Módulo elástico of 2.37 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 89 MPa Show Material materials with Resistencia a la flexión of 89 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 55 MPa Show Material materials with Resistencia a la tracción of 55 MPa | ASTM D 638 | Type I, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A |
-10.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | |
23.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.04E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.04E-4 1/K | ASTM E 831 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.04E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1.04E-4 1/K | ASTM E 831 | -40°C to 40°C |
Conductividad térmica | 23.0 °C | 0.23 W/(m·K) Show Material materials with Conductividad térmica of 0.23 W/(m·K) | ISO 8302 |
Heat deflection temperature, 1.80 MPa | 104 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 104 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |
Temperatura de fusión | 250 - 270 °C Show Material materials with Temperatura de fusión of 250 - 270 °C | ||
Temperatura de reblandecimiento Vicat | 123 °C Show Material materials with Temperatura de reblandecimiento Vicat of 123 °C | ASTM D 1525 | Rate B/50 |
Óptico
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.8 % Show Material materials with Contracción of 0.5 - 0.8 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.5 - 0.8 % Show Material materials with Contracción transversal of 0.5 - 0.8 % | SABIC method |
Velocidad de flujo de la masa derretida | 4 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 4 g/10min | ASTM D 1238 | 265°C/2.16kgf | |
Velocidad de flujo del volumen derretido | 3 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 3 cm³/10min | ISO 1133 | 265°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components | |
Processing methods | Drying Temperature: 75-90°C, Drying Time: 4-6hrs, Drying Time (Cumulative): 24hrs, Maximum Moisture Content: 0.01-0.02%, Barrel - Zone 1 Temperature: 235-260°C, Barrel - Zone 2 Temperature: 235-260°C, Barrel - Zone 3 Temperature: 235-260°C, Barrel - Zone 4 Temperature: 235-260°C, Adapter - Zone 5 Temperature: 235-260°C, Head - Zone 6 - Top Temperature: 240-270°C, Head - Zone 7 - Middle Temperature: 240-270°C, Head - Zone 7 - Bottom Temperature: 240-270°C, Mold Temperature: 30-75°C |