General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.25 % Show Material materials with Absorción de agua of 0.25 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.15 g/cm³ Show Material materials with Densidad of 1.15 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 35 % Show Material materials with Elongación of 35 % | ISO 527 | 50 mm/min |
Elongation at yield | 23.0 °C | 4.5 % Show Material materials with Elongation at yield of 4.5 % | ISO 527 | 50 mm/min |
Flexural yield strength | 23.0 °C | 80 MPa Show Material materials with Flexural yield strength of 80 MPa | ISO 178 | 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 98 MPa Show Material materials with Hardness, Ball Indentation of 98 MPa | ISO 2039-1 |
Límite elástico | 23.0 °C | 57 MPa Show Material materials with Límite elástico of 57 MPa | ISO 527 | 50 mm/min |
Módulo de flexión | 23.0 °C | 2.5 GPa Show Material materials with Módulo de flexión of 2.5 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.4 GPa Show Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min |
Resistencia a la tracción | 23.0 °C | 50 MPa Show Material materials with Resistencia a la tracción of 50 MPa | ISO 527 | 50 mm/min |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A |
23.0 °C | 33 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 33 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 - 0.6 % Show Material materials with Contracción of 0.4 - 0.6 % | SABIC method |
Velocidad de flujo del volumen derretido | 15 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | ISO 1133 | 260°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Applique,Audio,Auto Aftermarket,Building Element,Cluster,Cowl Vent Grille,Data Management,Data Transfer,Document Handling,Door Handle,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Exercise Equipment,Exterior Mirror,Exterior Trim,Exterior,Food Processor,Forward Lighting,Front Grille,Glove Box,Heavy Vehicles,Infotainment/Telematic,Interior,Lighting,Non-LED Lighting,Overhead,Personal Computing,Rear/Signal Lighting,Recreational Vehicle,Seat,Security/Detection,Spoiler,Trim,Wireless Communications | |
Processing methods | Drying Temperature: 90-105°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.04%, Melt Temperature: 260-275°C, Mold Temperature: 50-70°C |