General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Material materials with Absorción de agua of 0.15 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.34 g/cm³ Show Material materials with Densidad of 1.34 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 110 % Show Material materials with Elongación of 110 % | ASTM D 638 | Type I, 50 mm/min | ||
Elongation at yield | 23.0 °C | 5 % Show Material materials with Elongation at yield of 5 % | ASTM D 638 | Type I, 50 mm/min | ||
Flexural yield strength | 23.0 °C | 83 MPa Show Material materials with Flexural yield strength of 83 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span | ||
Hardness, Rockwell R | 23.0 °C | 117 [-] Show Material materials with Hardness, Rockwell R of 117 [-] | ASTM D 785 | ||
Impact strength, Izod notched, ASTM | -30.0 °C | 153 J/m Show Material materials with Impact strength, Izod notched, ASTM of 153 J/m | ASTM D 256 | ||
23.0 °C | 534 J/m Show Material materials with Impact strength, Izod notched, ASTM of 534 J/m | ASTM D 256 | |||
Límite elástico | 23.0 °C | 48 MPa Show Material materials with Límite elástico of 48 MPa | ASTM D 638 | Type I, 50 mm/min | ||
Módulo de flexión | 23.0 °C | 2.06 GPa Show Material materials with Módulo de flexión of 2.06 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span | ||
Módulo elástico | 23.0 °C | 2.02 GPa Show Material materials with Módulo elástico of 2.02 GPa | ASTM D 638 | 5 mm/min | ||
Resistencia a la flexión | 23.0 °C | 83 MPa Show Material materials with Resistencia a la flexión of 83 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span | ||
Resistencia a la tracción | 23.0 °C | 45 MPa Show Material materials with Resistencia a la tracción of 45 MPa | ASTM D 638 | Type I, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 45 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 45 kJ/m² | ISO 179/1eA | ||
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | ||
23.0 °C | 45 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 45 kJ/m² | ISO 180/1A | |||
Impact strength, Izod unnotched, ASTM | No break @ 23°C | ASTM D 4812 | ||||
Resistencia al choque, ensayo Charpy no entallado | No break @ 23°C | ISO 179/1eU | ||||
Resistencia al choque, ensayo Izod no entallado | No break @ 23,-30°C | ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.24E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.24E-4 1/K | ASTM E 831 | 60°C to 138°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 8.4E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 125 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 125 °C | ISO 75/Bf | 0.45 MPa | |||
Relative temperature index, electrical | 120 °C Show Material materials with Relative temperature index, electrical of 120 °C | UL 746B | |||
Relative temperature index, mechanical impact | 120 °C Show Material materials with Relative temperature index, mechanical impact of 120 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 134 °C Show Material materials with Temperatura de reblandecimiento Vicat of 134 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94-5VA Flame Class Rating | 3mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.2 [-] Show Material materials with Constante dieléctrica of 3.2 [-] | ASTM D 150 | at 1 MHz |
Factor de disipación | 23.0 °C | 0.03 [-] Show Material materials with Factor de disipación of 0.03 [-] | ASTM D 150 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 18.5 kV/mm Show Material materials with Rigidez dieléctrica of 18.5 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Material materials with Índice de seguimiento comparativo of 2 V | UL 746A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1 - 1.4 % Show Material materials with Contracción of 1 - 1.4 % | SABIC method | 2.3-4.6 mm |
Contracción transversal | 23.0 °C | 1.2 - 1.6 % Show Material materials with Contracción transversal of 1.2 - 1.6 % | SABIC method | 2.3-4.6 mm |
Velocidad de flujo de la masa derretida | 9.6 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 9.6 g/10min | ASTM D 1238 | 250°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 8 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 8 cm³/10min | ISO 1133 | 250°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning,Amusement Machine,Audio,Building Accessory,Circuit Protection,Cooking Range,Data Transfer,Defense Vehicles,Dishwasher,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Fluid Delivery,Food Processor,Freezer,Gas/Electric Oven,Golf Cart,Heavy Vehicles,Industrial Material Handling,Lab Ware and Clinical Diagnostics,Laundry Dryer,LED Lighting,Medical Device,Medical Facility Infrastructure,Non-LED Lighting,Oil/Gas,Personal Computing,Photovoltaic Components,Power Manangement,Pump,Recreational Vehicle,Refrigerator,Respiratory,Semiconductor,Small Appliance,Surgical Devices,Swimming Pool/Spa,Window,Wireless Communications,Wiring Devices,Wire & cable | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-265°C, Nozzle Temperature: 245-260°C, Front - Zone 3 Temperature: 250-265°C, Middle - Zone 2 Temperature: 245-260°C, Rear - Zone 1 Temperature: 240-255°C, Mold Temperature: 50-75°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-100rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.025-0.038mm |