General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.4 % Show Material materials with Absorción de agua of 0.4 % | Sim. to ISO 62 | 80mil |
Densidad | 23.0 °C | 1.31 g/cm³ Show Material materials with Densidad of 1.31 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.38 [-] Show Material materials with Coeficiente de Poisson of 0.38 [-] | |||
Elongación | 23.0 °C | 30 % Show Material materials with Elongación of 30 % | ISO 527-1/-2 | 50mm/min | ||
Elongation at yield | 23.0 °C | 10 % Show Material materials with Elongation at yield of 10 % | ISO 527-1/-2 | ||
Límite elástico | 23.0 °C | 58 MPa Show Material materials with Límite elástico of 58 MPa | ISO 527-1/-2 | ||
Módulo de flexión | 23.0 °C | 2.5 GPa Show Material materials with Módulo de flexión of 2.5 GPa | ISO 178 | ||
Módulo elástico | 23.0 °C | 2.7 GPa Show Material materials with Módulo elástico of 2.7 GPa | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 4 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break @ 23°C, ISO 179/1eU |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Calor específico | 23.0 °C | 2110 J/(kg·K) Show Material materials with Calor específico of 2110 J/(kg·K) | of melt | ||
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-4 1/K | ISO 11359-1/-2 | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.2E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1.2E-4 1/K | ISO 11359-1/-2 | ||
Heat deflection temperature, 1.80 MPa | 57 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 57 °C | ISO 75-1/-2 | |||
Temperatura de fusión | 225 °C Show Material materials with Temperatura de fusión of 225 °C | ISO 11357-1/-3 | 18°F/min | |||
Temperatura de transición del vidrio | 55 °C Show Material materials with Temperatura de transición del vidrio of 55 °C | ISO 11357-1/-2 | 18°F/min | |||
Inflamabilidad | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, Oxygen index: 22 %, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.8 % Show Material materials with Contracción of 1.8 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 1.8 % Show Material materials with Contracción transversal of 1.8 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 36 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 36 g/10min | ISO 1133 | 250°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 120°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.04%, Melt Temperature Optimum: 250°C, Min. melt temperature: 240°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 80°C, Min. mold temperature: 30°C, Max. mold temperature: 130°C, Hold pressure range: ≥60MPa, Hold pressure time: 4s/mm, Back pressure: As low as possible, Ejection temperature: 170°C |