General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.42 g/cm³ Show Material materials with Densidad of 1.42 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | |
Dureza Rockwell M | 23.0 °C | 94 [-] Show Material materials with Dureza Rockwell M of 94 [-] | ISO 2039-2 |
Elongación | 23.0 °C | 40 % Show Material materials with Elongación of 40 % | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 22 % Show Material materials with Elongation at yield of 22 % | ISO 527-1/-2 |
Hardness, Rockwell R | 23.0 °C | 122 [-] Show Material materials with Hardness, Rockwell R of 122 [-] | ISO 2039-2 |
Límite elástico | 23.0 °C | 73 MPa Show Material materials with Límite elástico of 73 MPa | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 2.9 GPa Show Material materials with Módulo de flexión of 2.9 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 3.1 GPa Show Material materials with Módulo elástico of 3.1 GPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -6.0 °C | 9 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | ISO 179/1eA |
23.0 °C | 10.5 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10.5 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 10 kJ/m² | ISO 180/1A |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-4 1/K | ISO 11359-1/-2 | 23 - 55°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.6E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1.6E-4 1/K | ISO 11359-1/-2 | 55 - 160°C | ||
Heat deflection temperature, 0.45 MPa | 165 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 165 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 99 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 99 °C | ISO 75-1/-2 | |||
Relative temperature index, electrical | 50 °C Show Material materials with Relative temperature index, electrical of 50 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical impact | 50 °C Show Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical strength | 50 °C Show Material materials with Relative temperature index, mechanical strength of 50 °C | UL 746B | 120mil | |||
Temperatura de fusión | 178 °C Show Material materials with Temperatura de fusión of 178 °C | ISO 11357-1/-3 | 18°F/min | |||
Inflamabilidad | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1MHz | 23.0 °C | 6E-3 [-] Show Material materials with Dissipation factor, 1MHz of 6E-3 [-] | IEC 62631-2-1 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.8 % Show Material materials with Contracción of 1.8 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 2 % Show Material materials with Contracción transversal of 2 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 2.3 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 2.3 g/10min | ISO 1133 | 190°C/2.16kg | |
Velocidad de flujo del volumen derretido | 1.9 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 1.9 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 215°C, Min. melt temperature: 210°C, Max. melt temperature: 220°C, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 90-110MPa, Hold pressure time: 7.5s/mm |