General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.42 g/cm³ Show Material materials with Densidad of 1.42 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | |||
Elongación | 23.0 °C | 40 % Show Material materials with Elongación of 40 % | ISO 527-1/-2 | ||
Elongation at yield | 23.0 °C | 22 % Show Material materials with Elongation at yield of 22 % | ISO 527-1/-2 | ||
Límite elástico | 23.0 °C | 71 MPa Show Material materials with Límite elástico of 71 MPa | ISO 527-1/-2 | ||
Módulo elástico | 23.0 °C | 3.05 GPa Show Material materials with Módulo elástico of 3.05 GPa | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -6.0 °C | 9.5 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 9.5 kJ/m² | ISO 179/1eA | ||
23.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | No Break @ 23,-6°C, ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 163 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 163 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 100 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 100 °C | ISO 75-1/-2 | |
Temperatura de fusión | 178 °C Show Material materials with Temperatura de fusión of 178 °C | ISO 11357-1/-3 | 18°F/min | |
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 2.1 % Show Material materials with Contracción of 2.1 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 1.8 % Show Material materials with Contracción transversal of 1.8 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 7 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 7 g/10min | ISO 1133 | 190°C/2.16kg | |
Velocidad de flujo del volumen derretido | 6 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 6 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 215°C, Min. melt temperature: 210°C, Max. melt temperature: 220°C, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 80-100MPa, Hold pressure time: 8s/mm |