Delrin® SC690 NC010

Want to keep this datasheet? Save it now in your required format

Description

Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades. Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.Delrin® SC690 is a low viscosity acetal homopolymer, developed for thin-walled parts requiring high precision molding in the healthcare industry.SPECIAL CONTROL for HEALTHCARE APPLICATIONSThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in Europe and the USA when meeting applicable use conditions. This product is also tested against ISO 10993-5 and -11 and selected parts of USP Class VI. For details, individual compliance statements are available from your DuPont representative.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Absorción de agua

23.0 °C

1.4 %

Show Material materials with Absorción de agua of 1.4 %

Sim. to ISO 62 | 80mil

Densidad

23.0 °C

1.42 g/cm³

Show Material materials with Densidad of 1.42 g/cm³

ISO 1183

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.37 [-]

Show Material materials with Coeficiente de Poisson of 0.37 [-]

Dureza Rockwell M

23.0 °C

92 [-]

Show Material materials with Dureza Rockwell M of 92 [-]

ISO 2039-2

Elongación

23.0 °C

23 %

Show Material materials with Elongación of 23 %

ISO 527-1/-2

Elongation at yield

23.0 °C

12 %

Show Material materials with Elongation at yield of 12 %

ISO 527-1/-2

Hardness, Rockwell R

23.0 °C

120 [-]

Show Material materials with Hardness, Rockwell R of 120 [-]

ISO 2039-2

Límite elástico

23.0 °C

71 MPa

Show Material materials with Límite elástico of 71 MPa

ISO 527-1/-2

Módulo de flexión

23.0 °C

3 GPa

Show Material materials with Módulo de flexión of 3 GPa

ISO 178

Módulo elástico

23.0 °C

3.3 GPa

Show Material materials with Módulo elástico of 3.3 GPa

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

-6.0 °C

7 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m²

ISO 179/1eA

23.0 °C

8 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m²

ISO 179/1eA

Resistencia al choque, ensayo Charpy no entallado

-6.0 °C

200 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 200 kJ/m²

ISO 179/1eU

23.0 °C

200 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 200 kJ/m²

ISO 179/1eU

Unlock all property charts

Resistencia al choque, ensayo Izod no entallado

-40.0 °C

8 kJ/m²

Show Material materials with Resistencia al choque, ensayo Izod no entallado of 8 kJ/m²

ISO 180/1A

23.0 °C

7 kJ/m²

Show Material materials with Resistencia al choque, ensayo Izod no entallado of 7 kJ/m²

ISO 180/1A

Unlock all property charts

Aplicaciones térmicas

PropertyTemperatureValueComment

Coeficiente de dilatación térmica

23.0 °C

1E-4 1/K

Show Material materials with Coeficiente de dilatación térmica of 1E-4 1/K

ASTM E 831 | 55 - 160°C

Coeficiente de dilatación térmica transversal

23.0 °C

1.2E-4 1/K

Show Material materials with Coeficiente de dilatación térmica transversal of 1.2E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

162 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 162 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

94 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 94 °C

ISO 75-1/-2

Relative temperature index, electrical

110 °C

Show Material materials with Relative temperature index, electrical of 110 °C

UL 746B | 120mil

Relative temperature index, mechanical impact

90 °C

Show Material materials with Relative temperature index, mechanical impact of 90 °C

UL 746B | 120mil

Relative temperature index, mechanical strength

95 °C

Show Material materials with Relative temperature index, mechanical strength of 95 °C

UL 746B | 120mil

Temperatura de fusión

178 °C

Show Material materials with Temperatura de fusión of 178 °C

ISO 11357-1/-3 | 18°F/min

Temperatura de reblandecimiento Vicat

160 °C

Show Material materials with Temperatura de reblandecimiento Vicat of 160 °C

ISO 306 | 90°F/h, 11 lbf

Inflamabilidad

Hot Wire Ignition, 30mil: 8 s

Eléctrico

PropertyTemperatureValueComment

Constante dieléctrica, 1 MHz

23.0 °C

3.8 [-]

Show Material materials with Constante dieléctrica, 1 MHz of 3.8 [-]

IEC 62631-2-1

Constante dieléctrica, 100 Hz

23.0 °C

3.8 [-]

Show Material materials with Constante dieléctrica, 100 Hz of 3.8 [-]

IEC 62631-2-1

Dissipation factor, 1MHz

23.0 °C

5E-3 [-]

Show Material materials with Dissipation factor, 1MHz of 5E-3 [-]

IEC 62631-2-1

Surface resistivity

23.0 °C

1.00E+15 Ω/sq

Show Material materials with Surface resistivity of 1.00E+15 Ω/sq

min. | IEC 62631-3-2

Volume resistivity

23.0 °C

1.00E+14 Ω·cm

Show Material materials with Volume resistivity of 1.00E+14 Ω·cm

IEC 62631-3-1

Índice de seguimiento comparativo

23.0 °C

600 V

Show Material materials with Índice de seguimiento comparativo of 600 V

IEC 60112

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

1.9 %

Show Material materials with Contracción of 1.9 %

ISO 294-4, 2577

Contracción transversal

23.0 °C

1.9 %

Show Material materials with Contracción transversal of 1.9 %

ISO 294-4, 2577

Velocidad de flujo de la masa derretida

25 g/10min

Show Material materials with Velocidad de flujo de la masa derretida of 25 g/10min

ISO 1133 | 190°C/2.16kg

Velocidad de flujo del volumen derretido

21 cm³/10min

Show Material materials with Velocidad de flujo del volumen derretido of 21 cm³/10min

ISO 1133

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 215°C, Min. melt temperature: 210°C, Max. melt temperature: 220°C, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 80-100MPa, Hold pressure time: 8s/mm