General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.42 g/cm³ Show Material materials with Densidad of 1.42 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | |
Elongation at yield | 23.0 °C | 10 % Show Material materials with Elongation at yield of 10 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 72 MPa Show Material materials with Límite elástico of 72 MPa | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 3.1 GPa Show Material materials with Módulo de flexión of 3.1 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 3.4 GPa Show Material materials with Módulo elástico of 3.4 GPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 4 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | ISO 179/1eA |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 2 % Show Material materials with Contracción of 2 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 2 % Show Material materials with Contracción transversal of 2 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 22 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 22 g/10min | ISO 1133 | 190°C/2.16kg | |
Velocidad de flujo del volumen derretido | 19 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 19 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 215°C, Min. melt temperature: 210°C, Max. melt temperature: 220°C, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 80-100MPa, Hold pressure time: 7.5s/mm |