General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.45 g/cm³ Show Material materials with Densidad of 1.45 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | |
Elongación | 23.0 °C | 2.5 % Show Material materials with Elongación of 2.5 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 7 GPa Show Material materials with Módulo de flexión of 7 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 7.5 GPa Show Material materials with Módulo elástico of 7.5 GPa | ISO 527-1/-2 |
Resistencia a la tracción | 23.0 °C | 120 MPa Show Material materials with Resistencia a la tracción of 120 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 3 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Izod no entallado | -40.0 °C | 3.4 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 3.4 kJ/m² | ISO 180/1A |
23.0 °C | 4 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 4 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 4.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 4.1E-5 1/K | ISO 11359-1/-2 | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 6.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 6.2E-5 1/K | ISO 11359-1/-2 | ||
Heat deflection temperature, 0.45 MPa | 255 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 255 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 230 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 230 °C | ISO 75-1/-2 | |||
Relative temperature index, electrical | 65 °C Show Material materials with Relative temperature index, electrical of 65 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical impact | 65 °C Show Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical strength | 65 °C Show Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | 120mil | |||
Temperatura de fusión | 263 °C Show Material materials with Temperatura de fusión of 263 °C | ISO 11357-1/-3 | 18°F/min | |||
Inflamabilidad | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 0.81 mm, UL recognition: yes -, FMVSS Class: SE -, Burning rate, Thickness 1 mm: 23 mm/min |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 475 V Show Material materials with Índice de seguimiento comparativo of 475 V | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 38% Glass Fiber and Mineral Powder | |
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 295°C, Min. melt temperature: 285°C, Max. melt temperature: 305°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C |