General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.38 g/cm³ Show Material materials with Densidad of 1.38 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.36 [-] Show Material materials with Coeficiente de Poisson of 0.36 [-] | |
Elongación | 23.0 °C | 15 % Show Material materials with Elongación of 15 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 4.4 GPa Show Material materials with Módulo de flexión of 4.4 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 4.8 GPa Show Material materials with Módulo elástico of 4.8 GPa | ISO 527-1/-2 |
Resistencia a la tracción | 23.0 °C | 78 MPa Show Material materials with Resistencia a la tracción of 78 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -40.0 °C | 4 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | ISO 179/1eA |
-6.0 °C | 5 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | ISO 179/1eA | |
23.0 °C | 7 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -6.0 °C | 75 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | ISO 179/1eU |
23.0 °C | 120 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 120 kJ/m² | ISO 179/1eU | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 85 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 85 kJ/m² | ISO 180/1U |
23.0 °C | 110 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 110 kJ/m² | ISO 180/1U | |
Resistencia al choque, ensayo Izod no entallado | -40.0 °C | 5 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 5 kJ/m² | ISO 180/1A |
-30.0 °C | 6 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 6 kJ/m² | ISO 180/1A | |
23.0 °C | 7 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 7 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 215 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 215 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 80 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 80 °C | ISO 75-1/-2 | |
Temperatura de fusión | 257 °C Show Material materials with Temperatura de fusión of 257 °C | ISO 11357-1/-3 | 18°F/min | |
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property | ||
---|---|---|
Fillers | 32% Mineral Powder | |
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 295°C, Min. melt temperature: 285°C, Max. melt temperature: 305°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C |