General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 6 % Show Material materials with Absorción de agua of 6 % | Sim. to ISO 62 | 80mil |
Densidad | 23.0 °C | 1.37 g/cm³ Show Material materials with Densidad of 1.37 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | |
Elongación | 23.0 °C | 3 % Show Material materials with Elongación of 3 % | ISO 527-1/-2 |
Módulo elástico | 23.0 °C | 9 GPa Show Material materials with Módulo elástico of 9 GPa | ISO 527-1/-2 |
Resistencia a la tracción | 23.0 °C | 160 MPa Show Material materials with Resistencia a la tracción of 160 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 60 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | ISO 179/1eU |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Calor específico | 23.0 °C | 2290 J/(kg·K) Show Material materials with Calor específico of 2290 J/(kg·K) | of melt | ||
Difusividad térmica | 23.0 °C | 0 mm²/s Show Material materials with Difusividad térmica of 0 mm²/s | |||
Temperatura de fusión | 262 °C Show Material materials with Temperatura de fusión of 262 °C | ISO 11357-1/-3 | 18°F/min | |||
Temperatura de transición del vidrio | 80 °C Show Material materials with Temperatura de transición del vidrio of 80 °C | ISO 11357-1/-2 | 18°F/min | |||
Inflamabilidad | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, Burning Behav. at thickness h: HB class, Thickness tested: 0.75 mm, Oxygen index: 24 %, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 295°C, Min. melt temperature: 285°C, Max. melt temperature: 305°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C |