General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.04 g/cm³ Show Material materials with Densidad of 1.04 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.45 [-] Show Material materials with Coeficiente de Poisson of 0.45 [-] | |
Elongación | 23.0 °C | 500 % Show Material materials with Elongación of 500 % | min. | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.9 GPa Show Material materials with Módulo de flexión of 0.9 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 0.9 GPa Show Material materials with Módulo elástico of 0.9 GPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -40.0 °C | 30 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 30 kJ/m² | ISO 179/1eA |
23.0 °C | 105 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 105 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod no entallado | -40.0 °C | 25 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 25 kJ/m² | ISO 180/1A |
23.0 °C | 95 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 95 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 68 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 68 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 50 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 50 °C | ISO 75-1/-2 | |
Temperatura de fusión | 263 °C Show Material materials with Temperatura de fusión of 263 °C | ISO 11357-1/-3 | 18°F/min | |
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 285°C, Min. melt temperature: 275°C, Max. melt temperature: 295°C, Mold Temperature Optimum: 60°C, Min. mold temperature: 40°C, Max. mold temperature: 80°C |